| 性能項(xiàng)目 | 測(cè)試條件 | 測(cè)試方法 | 數(shù)值/描述 | 單位 | |
| 機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | kg/cm2(MPa)[Lb/in2] | ||
| 斷裂伸長(zhǎng)率 | ASTM D638/ISO 527 | % | |||
| 拉伸模量 | ASTM D638/ISO 527 | kg/cm2(MPa)[Lb/in2] | |||
| 拉伸屈服伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | % | |||
| 拉伸斷裂伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | % | |||
| 彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 14600 | kg/cm2(MPa)[Lb/in2] | ||
| 彎曲強(qiáng)度 | ASTM D790/ISO 178 | kg/cm2(MPa)[Lb/in2] | |||
| 洛氏硬度 | ASTM D785 | 81 | kg·cm/cm(J/M)ft·lb/in | ||
| IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
| 1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
| -30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 23℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| -30℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 0.897 | ||
| 成型收縮率 | ASTM D955 | 1.4 | % | ||
PP/李長(zhǎng)榮化工(福聚)/7433 高抗沖 嵌段共聚