| TYPICAL PROPERTIES (1) | 
		
			| MECHANICAL | Value | Unit | Standard | 
		
			| Tensile Stress, yld, Type I, 50 mm/min | 610 | kgf/cm2 | ASTM D 638 | 
		
			| Tensile Stress, brk, Type I, 50 mm/min | 400 | kgf/cm2 | ASTM D 638 | 
		
			| Tensile Strain, yld, Type I, 50 mm/min | 3 | % | ASTM D 638 | 
		
			| Tensile Strain, brk, Type I, 50 mm/min | 15 | % | ASTM D 638 | 
		
			| Tensile Modulus, 50 mm/min | 31600 | kgf/cm2 | ASTM D 638 | 
		
			| Tensile Stress, yield, 50 mm/min | 60 | MPa | ISO 527 | 
		
			| Tensile Stress, break, 50 mm/min | 50 | MPa | ISO 527 | 
		
			| Tensile Strain, yield, 50 mm/min | 3 | % | ISO 527 | 
		
			| Tensile Strain, break, 50 mm/min | >70 | % | ISO 527 | 
		
			| Tensile Modulus, 1 mm/min | 3200 | MPa | ISO 527 | 
		
			| Flexural Stress, yield, 2 mm/min | 95 | MPa | ISO 178 | 
		
			| Flexural Modulus, 2 mm/min | 2850 | MPa | ISO 178 | 
		
			| Hardness, H358/30 | 170 | MPa | ISO 2039-1 | 
		
			| Hardness, Rockwell R | 118 | - | ISO 2039-2 | 
		
			| IMPACT | Value | Unit | Standard | 
		
			| Charpy Impact, unnotched, 23°C | 95 | kJ/m2 | ISO 179/2C | 
		
			| Charpy Impact, unnotched, -30°C | 80 | kJ/m2 | ISO 179/2C | 
		
			| Izod Impact, unnotched, 23°C | 96 | cm-kgf/cm | ASTM D 4812 | 
		
			| Izod Impact, unnotched, -30°C | 84 | cm-kgf/cm | ASTM D 4812 | 
		
			| Izod Impact, notched, 23°C | 4 | cm-kgf/cm | ASTM D 256 | 
		
			| Izod Impact, notched, 0°C | 4 | cm-kgf/cm | ASTM D 256 | 
		
			| Izod Impact, notched, -30°C | 4 | cm-kgf/cm | ASTM D 256 | 
		
			| Izod Impact, unnotched 80*10*4 +23°C | 60 | kJ/m2 | ISO 180/1U | 
		
			| Izod Impact, unnotched 80*10*4 -30°C | 60 | kJ/m2 | ISO 180/1U | 
		
			| Izod Impact, notched 80*10*4 +23°C | 6 | kJ/m2 | ISO 180/1A | 
		
			| Izod Impact, notched 80*10*4 0°C | 6 | kJ/m2 | ISO 180/1A | 
		
			| Izod Impact, notched 80*10*4 -30°C | 6 | kJ/m2 | ISO 180/1A | 
		
			| Charpy 23°C, V-notch Edgew 80*10*4 sp=62mm | 5 | kJ/m2 | ISO 179/1eA | 
		
			| Charpy Impact, notched, 23°C | 6 | kJ/m2 | ISO 179/2C | 
		
			| Charpy Impact, notched, -30°C | 5 | kJ/m2 | ISO 179/2C | 
		
			| THERMAL | Value | Unit | Standard | 
		
			| Vicat Softening Temp, Rate A/50 | 220 | °C | ASTM D 1525 | 
		
			| Vicat Softening Temp, Rate B/50 | 180 | °C | ASTM D 1525 | 
		
			| HDT, 0.45 MPa, 3.2 mm, unannealed | 165 | °C | ASTM D 648 | 
		
			| HDT, 1.82 MPa, 3.2mm, unannealed | 80 | °C | ASTM D 648 | 
		
			| CTE, -40°C to 40°C, flow | 6.01E-05 | 1/°C | ISO 11359-2 | 
		
			| CTE, -40°C to 40°C, xflow | 7.4E-05 | 1/°C | ISO 11359-2 | 
		
			| CTE, 23°C to 150°C, flow | 1.9E-04 | 1/°C | ISO 11359-2 | 
		
			| CTE, 23°C to 150°C, xflow | 1.42E-04 | 1/°C | ISO 11359-2 | 
		
			| Ball Pressure Test, 125°C +/- 2°C | PASSES | - | IEC 60695-10-2 | 
		
			| Vicat Softening Temp, Rate A/50 | 220 | °C | ISO 306 | 
		
			| Vicat Softening Temp, Rate B/50 | 180 | °C | ISO 306 | 
		
			| Vicat Softening Temp, Rate B/120 | 180 | °C | ISO 306 | 
		
			| HDT/Bf, 0.45 MPa Flatw 80*10*4 sp=64mm | 165 | °C | ISO 75/Bf | 
		
			| HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm | 80 | °C | ISO 75/Af | 
		
			| Relative Temp Index, Elec | 75 | °C | UL 746B | 
		
			| Relative Temp Index, Mech w/impact | 75 | °C | UL 746B | 
		
			| Relative Temp Index, Mech w/o impact | 75 | °C | UL 746B | 
		
			| PHYSICAL | Value | Unit | Standard | 
		
			| Specific Gravity | 1.5 | - | ASTM D 792 | 
		
			| Mold Shrinkage on Tensile Bar, flow (2) (5) | 1.1 - 1.8 | % | SABIC Method | 
		
			| Mold Shrinkage on Tensile Bar, xflow (2) (5) | 0.9 - 1.8 | % | SABIC Method | 
		
			| Melt Flow Rate, 265°C/5.0 kgf | 50 | g/10 min | ASTM D 1238 | 
		
			| Melt Flow Rate, 266°C/5.0 kgf | 50 | g/10 min | ASTM D 1238 | 
		
			| Density | 1.5 | g/cm3 | ISO 1183 | 
		
			| Water Absorption, (23°C/sat) | 0.35 | % | ISO 62 | 
		
			| Moisture Absorption (23°C / 50% RH) | 0.08 | % | ISO 62 | 
		
			| Melt Volume Rate, MVR at 250°C/2.16 kg | 13 | cm3/10 min | ISO 1133 | 
		
			| Melt Volume Rate, MVR at 250°C/5.0 kg | 13 | cm3/10 min | ISO 1133 | 
		
			| Melt Volume Rate, MVR at 265°C/5.0 kg | 40 | cm3/10 min | ISO 1133 | 
		
			| Melt Viscosity, 260°C, 1500 sec-1 | 170 | Pa-s | ISO 11443 | 
		
			| ELECTRICAL | Value | Unit | Standard | 
		
			| Volume Resistivity | >1.E+15 | Ohm-cm | ASTM D 257 | 
		
			| Dielectric Strength, in oil, 1.6 mm | 39 | kV/mm | ASTM D 149 | 
		
			| Dielectric Strength, in oil, 3.2 mm | 21 | kV/mm | ASTM D 149 | 
		
			| Relative Permittivity, 1 MHz | 2.9 | - | ASTM D 150 | 
		
			| Dissipation Factor, 1 MHz | 0.016 | - | ASTM D 150 | 
		
			| Volume Resistivity | >1.E+15 | Ohm-cm | IEC 60093 | 
		
			| Surface Resistivity, ROA | >1.E+15 | Ohm | IEC 60093 | 
		
			| Dielectric Strength, in oil, 0.8 mm | 62 | kV/mm | IEC 60243-1 | 
		
			| Dielectric Strength, in oil, 1.6 mm | 39 | kV/mm | IEC 60243-1 | 
		
			| Dielectric Strength, in oil, 3.2 mm | 21 | kV/mm | IEC 60243-1 | 
		
			| Relative Permittivity, 1 MHz | 2.9 | - | IEC 60250 | 
		
			| Dissipation Factor, 1 MHz | 0.016 | - | IEC 60250 | 
		
			| Comparative Tracking Index | 225 | V | IEC 60112 | 
		
			| FLAME CHARACTERISTICS | Value | Unit | Standard | 
		
			| UL Compliant, 94V-0 Flame Class Rating (3)(4) | 0.8 | mm | UL 94 by SABIC-IP |